SpecificationTest Parameters
Solderability: Solder coverage 90% of metalized areas. Preheat chip to 120°-150°C for 60 sec.
Dip terminals in rosin flux then dip in 62Sn/36Pb/2Ag solder @ 240±5°C
Dip time = 5±1 sec.
Resistance to Soldering Heat:

Chip should not crack.
Solder coverage 80%

Preheat chip to 120°-150°C for 60 sec.
Dip terminals in rosin flux then dip in 62Sn/36Pb/2Ag solder @ 260¡±5°C
Dip time = 10±1 sec.
Terminal Adhesion: Termination should not pull off.
Ceramic should remain undamaged.
Linear pull force exerted on axial leads soldered to each terminal. Terminal strength: 2.0Lbs for 0403, 2.0Lbs for 0504, 6.0Lbs for 1210
PCB Deflection: No mechanical damage.
Cap. change: 2% or .5pF Max
Glass Epoxy PCB: 1 mm deflection
Life Test: Cap. change: 2% or .5pF Max
I.R. = Initial value
1000 Hours, 125°C, 200% rated voltage
Thermal Shock: I.R. = 70% of initial value 5 CYCLES: 30±3 minutes @ -55°C, 3 min. @ 25°C, 30±3 min. @ +125°C, 3 min. @ 25°C
Moisture Resistance: Cap. change: 2% or .5pF Max
I.R. = 70% of initial value
240 Hours, 85% Relative Humidity, 85°C, 1.5 VDC

 

Obsolete - No longer available


<< Return to Porcelain Substitute NPO Ceramic Caps Overview

 
 
 

Part Locator

About Us
Contact Us
Sales Reps
Distributors
Prototyping Kits
Cross Reference Charts
Designer Libraries
Modeling Software
Sitemap Johanson Technology, Inc.
4001 Calle Tecate
Camarillo, CA 93012
(805) 389-1166 phone
(805) 389-1821 fax
Copyright © 2012 Johanson Technology   All rights reserved.